| Grade Name | Polymer | Product Short Description |
|
Crastin® 6129 NC010 |
PBT |
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Moulding |
|
Crastin® 6130 NC010 |
PBT |
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Moulding |
|
Crastin® 6131 NC010 |
PBT |
Unreinforced Low Viscosity Polybutylene Terephthalate |
|
Crastin® 6134 NC010 |
PBT |
Unreinforced Medium Viscosity Polybutylene Terephthalate |
|
Crastin® BM6450XD BK560 |
PBT |
Unreinforced Polybutylene Terephthalate Developed for Blow Moulding |
|
Crastin® CE15315 BK010 |
PBT-GF15 FR(17) |
15% Glass Reinforced, Flame Retardant, Polybutylene Terephthalate |
|
Crastin® CE15315 NC010 |
PBT-GF15 FR(17) |
15% Glass Reinforced, Flame Retardant, Polybutylene Terephthalate |
|
Crastin® CE15330 BK010 |
PBT-GF30 FR(17) |
30% Glass Reinforced, Flame Retardant, Polybutylene Terephthalate |
|
Crastin® CE15330 NC010 |
PBT-GF30 FR(17) |
30% Glass Reinforced, Flame Retardant, Polybutylene Terephthalate |
|
Crastin® CE3054 BK580 |
PBT |
||
Crastin® FG6130 NC010 |
PBT |
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Food Contact Applications and Extrusion and Injection Moulding |
|
Crastin® FG6134 NC010 |
PBT |
Unreinforced Medium Viscosity Polybutylene Terephthalate Developed for Food Contact Applications |
|
Crastin® FGS600F10 NC010 |
PBT |
Unreinforced Polybutylene Terephthalate Developed for Food Contact Applications |
|
Crastin® FGS600F40 BK594 |
PBT |
||
Crastin® FGS600F40 NC010 |
PBT |
Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Food Contact Applications |
|
Crastin® HR5315HF BK503 |
PBT-I-GF15 |
15% Glass Reinforced, Hydrolysis Resistant, Polybutylene Terephthalate |
|
Crastin® HR5315HF NC010 |
PBT-I-GF15 |
15% Glass Reinforced, Hydrolysis Resistant, Polybutylene Terephthalate |
|
Crastin® HR5315HFS BK591 |
PBT-I-GF15 |
15% Glass Reinforced, Hydrolysis Resistant, Laser Markable Polybutylene Terephthalate with Improved Processing |
|
Crastin® HR5315HFS NC010 |
PBT-I-GF15 |
15% Glass Reinforced, Hydrolysis Resistant, Polybutylene Terephthalate with Improved Processing |
|
Crastin® HR5330HF BK503 |
PBT-I-GF30 |
30% Glass Reinforced, Hydrolysis Resistant, Polybutylene Terephthalate |
|
Crastin® HR5330HF NC010 |
PBT-I-GF30 |
30% Glass Reinforced, Hydrolysis Resistant, Polybutylene Terephthalate |
|
Crastin® HR5330HFS BK591 |
PBT-I-GF30 |
30% Glass Reinforced, Hydrolysis Resistant, Laser Markable Polybutylene Terephthalate with Improved Processing |
|
Crastin® HR5330HFS NC010 |
PBT-I-GF30 |
30% Glass Reinforced Polybutylene Terephthalate with Improved Processing |
|
Crastin® LW9020 BK580 |
(PBT+ASA)-GF20 |
20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics |
|
Crastin® LW9020 NC010 |
(PBT+ASA)-GF20 |
20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics |
|
Crastin® LW9020FR BK851 |
(PBT+ASA)-GF20 FR(17) |
20% Glass Reinforced, Flame Retardant, Polybutylene Terephthalate Blend with Low Warpage Characteristics |
|
Crastin® LW9030 BK851 |
(PBT+ASA)-GF30 |
30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics |
|
Crastin® LW9030 NC010 |
(PBT+ASA)-GF30 |
30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics |
|
Crastin® LW9030FR BK851 |
(PBT+ASA)-GF30 FR(17) |
30% Glass Reinforced, Flame Retardant, Polybutylene Terephthalate Blend with Low Warpage Characteristics |
|
Crastin® LW9030FR NC010 |
(PBT+ASA)-GF30 FR(17) |
30% Glass Reinforced, Flame Retardant, Polybutylene Terephthalate Blend with Low Warpage Characteristics |
|
Crastin® LW9320 BK851 |
(PBT+SAN)-I-GF20 |
20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics |
|
Crastin® LW9320 NC010 |
(PBT+SAN)-I-GF20 |
20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics |
|
Crastin® LW9320LM BK591 |
(PBT+SAN)-I-GF20 |
20% Glass Reinforced Laser Markable Polybutylene Terephthalate Blend with Low Warpage Characteristics |
|
Crastin® LW9330 BK851 |
(PBT+SAN)-I-GF30 |
30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics |
|
Crastin® LW9330 NC010 |
(PBT+SAN)-I-GF30 |
30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics |
|
Crastin® PC164 NC010 |
PBT |
Unreinforced Polybutylene Terephthalate |
|
Crastin® S600F10 BK851 |
PBT |
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Moulding |
|
Crastin® S600F10 NC010 |
PBT |
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Moulding |
|
Crastin® S600F20 BK851 |
PBT |
Unreinforced Medium Viscosity Polybutylene Terephthalate |
|
Crastin® S600F20 NC010 |
PBT |
Unreinforced Medium Viscosity Polybutylene Terephthalate |
|
Crastin® S600F40 BK851 |
PBT |
Unreinforced Low Viscosity Polybutylene Terephthalate |
|
Crastin® S600F40 NC010 |
PBT |
Unreinforced Low Viscosity Polybutylene Terephthalate |
|
Crastin® S610SF NC010 |
PBT |
Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production |
|
Crastin® S620F20 BK851 |
PBT |
Unreinforced Medium Viscosity Polybutylene Terephthalate |
|
Crastin® S620F20 NC010 |
PBT |
Unreinforced Medium Viscosity Polybutylene Terephthalate |
|
Crastin® S650FR NC010 |
PBT FR(17) |
Unreinforced, Flame Retardant, Polybutylene Terephthalate |
|
Crastin® SC164 NC010 |
PBT |
Unreinforced Polybutylene Terephthalate |
|
Crastin® SC193 NC010 |
(PBT+SAN)-GF30 |
30% Glass Reinforced Polybutylene Terephthalate Blend Developed for Healthcare Industry |
|
Crastin® SK601 BK851 |
PBT-GF10 |
10% Glass Reinforced Polybutylene Terephthalate |
|
Crastin® SK601 NC010 |
PBT-GF10 |
10% Glass Reinforced Polybutylene Terephthalate |
|
Crastin® SK602 BK851 |
PBT-GF15 |
15% Glass Reinforced Polybutylene Terephthalate |
|
Crastin® SK602 NC010 |
PBT-GF15 |
15% Glass Reinforced Polybutylene Terephthalate |
|
Crastin® SK603 BK851 |
PBT-GF20 |
20% Glass Reinforced Polybutylene Terephthalate |
|
Crastin® SK603 NC010 |
PBT-GF20 |
20% Glass Reinforced Polybutylene Terephthalate |
|
Crastin® SK605 BK851 |
PBT-GF30 |
30% Glass Reinforced Polybutylene Terephthalate |
|
Crastin® SK605 NC010 |
PBT-GF30 |
30% Glass Reinforced Polybutylene Terephthalate |
|
Crastin® SK605LM BK591 |
PBT-GF30 |
30% Glass Reinforced, Laser Markable, Polybutylene Terephthalate |
|
Crastin® SK608 BK509 |
PBT-GF45 |
45% Glass Reinforced Polybutylene Terephthalate |
|
Crastin® SK609 BK851 |
PBT-GF50 |
50% Glass Reinforced Polybutylene Terephthalate |
|
Crastin® SK609 NC010 |
PBT-GF50 |
50% Glass Reinforced Polybutylene Terephthalate |
|
Crastin® SK612SF NC010 |
PBT-GF15 |
15% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production |
|
Crastin® SK615SF BK591 |
PBT-GF30 |
30% Glass Reinforced Low Viscosity Laser Markable Polybutylene Terephthalate Developed for Super Fast Production |
|
Crastin® SK615SF NC010 |
PBT-GF30 |
30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production |
|
Crastin® SK643FR BK851 |
PBT-GF20 FR(17) |
20% Glass Reinforced, Flame Retardant, Polybutylene Terephthalate |
|
Crastin® SK645FR BK851 |
PBT-GF30 FR(17) |
30% Glass Reinforced, Flame Retardant, Polybutylene Terephthalate |
|
Crastin® SK645FR NC010 |
PBT-GF30 FR(17) |
30% Glass Reinforced, Flame Retardant, Polybutylene Terephthalate |
|
Crastin® SK692FR BK507 |
PBT-GF15 FR(17) |
15% Glass Reinforced, Flame Retardant, Polybutylene Terephthalate |
|
Crastin® SK692FR NC010 |
PBT-GF15 FR(17) |
15% Glass Reinforced, Flame Retardant, Polybutylene Terephthalate |
|
Crastin® SK695FR BK507 |
PBT-GF30 FR(17) |
30% Glass Reinforced, Flame Retardant, Polybutylene Terephthalate |
|
Crastin® SK695FR NC010 |
PBT-GF30 FR(17) |
30% Glass Reinforced, Flame Retardant, Polybutylene Terephthalate |
|
Crastin® SO653 NC010 |
PBT-GB20 |
20% Glass Bead Filled Polybutylene Terephthalate with Low Warpage Characteristics |
|
Crastin® ST820 BK503 |
PBT-I |
Unreinforced Polybutylene Terephthalate with Excellent Impact Resistance |
|
Crastin® ST820 NC010 |
PBT-I |
Unreinforced Polybutylene Terephthalate with Excellent Impact Resistance |
|
Crastin® ST830FRUV NC010 |
PBT-I FR(17) |
Unreinforced, Flame Retardant, UV Stabilised, Polybutylene Terephthalate |
|
Crastin® T841FR1 NC010 |
PBT-GF10 FR(17) |
10% Glass Reinforced, Flame Retardant, ToughenedPolybutylene Terephthalate |
|
Crastin® T843FR BK851 |
PBT-GF20 FR(17)... |
20% Glass Reinforced, Flame Retardant, Toughened, Polybutylene Terephthalate |
|
Crastin® T843FR NC010 |
PBT-GF20 FR(17) |
20% Glass Reinforced, Toughened, Flame Retardant, Polybutylene Terephthalate with Improved Impact Resistance |
|
Delrin® 100 BK602 |
POM |
High Viscosity Acetal Homopolymer |
|
Delrin® 100 NC010 |
POM |
High Viscosity Acetal Homopolymer |
|
Delrin® 100AF |
POM-Z20 |
20% Teflon® Fiber Filled High Viscosity Acetal Homopolymer with Low Wear and Low Friction |
|
Delrin® 100AL NC010 |
POM-Z |
Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction |
|
Delrin® 100ALE NC010 |
POM-Z |
||
Delrin® 100CPE NC010 |
POM |
High Viscosity Acetal Homopolymer with Very Low Emissions |
|
Delrin® 100KM NC000 |
POM-Z |
Kevlar® Modified High Viscosity Acetal Homopolymer with Low Wear and Low Friction |
|
Delrin® 100P BK602 |
POM |
High Viscosity Acetal Homopolymer with Improved Processing |
|
Delrin® 100P NC010 |
POM |
High Viscosity Acetal Homopolymer with Improved Processing |
|
Delrin® 100PE BK602 |
POM |
High Viscosity Acetal Homopolymer with Very Low Emissions |
|
Delrin® 100PE NC010 |
POM |
High Viscosity Acetal Homopolymer with Very Low Emissions |
|
Delrin® 100ST BK602 |
POM-I |
Super Toughened High Viscosity Acetal Homopolymer |
|
Delrin® 100ST NC010 |
POM-I |
Super Toughened High Viscosity Acetal Homopolymer |
|
Delrin® 100STE NC010 |
POM-I |
Super Toughened High Viscosity Acetal Homopolymer with Very Low Emissions |
|
Delrin® 100T BK602 |
POM-I |
Toughened High Viscosity Acetal Homopolymer |
|
Delrin® 100T NC010 |
POM-I |
Toughened High Viscosity Acetal Homopolymer |
|
Delrin® 100TE NC010 |
POM-I |
Toughened High Viscosity Acetal Homopolymer with Very Low Emissions |
|
Delrin® 100TL NC010 |
POM-Z |
Teflon® Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction |
|
Delrin® 111DP BK402 |
POM |
||
Delrin® 111DP NC010 |
POM |
Nucleated High Viscosity Acetal Homopolymer |
|
Delrin® 127UV BK701 |
POM |
UV Stabilised High Viscosity Acetal Homopolymer |
|
Delrin® 127UV NC010 |
POM |
UV Stabilised High Viscosity Acetal Homopolymer |
|
Delrin® 127UVE BK701 |
POM |
UV Stabilized High Viscosity Acetal Homopolymer with Very Low Emissions |

Please wait while loading data...